    Creep Testing Unit

    Specification
    [1] Table unit for the investigation of the creep behaviour of different materials
    [2] Flat specimens made of lead and PE
    [3] Specimen cross-section 2x5mm, measured length 25mm
    [4] Tensile stress range 5…25N/mm²
    [5] Position measurement gauge 0…10mm, resolution 0.01mm
    [6] Experiments above or below room temperature possible with conditioning box
    Technical Data
    Specimen
    – material: lead, PE
    – cross-section: 2x5mm
    – measured length: 25mm
    Tensile stress range: 5…25N/mm²
    Position measurement
    – range: 0…10mm
    – resolution 0.01mm